S355J0 – BS EN 10025-2:2004

S355J0 BS EN 10025-2:2004 Hot rolled products of structural steels Part 2: Technical delivery conditions for non-alloy structural steels Chemical composition of the ladle analysis of S355J0 Chemical composition of the prduct analysis of S355J0 Maximum CEV based on the ladle analysis of S355J0 Mechanical properties of S355J0 impact strength KV longitudinal S355J0  

ASTM A182 F904L

ASTM A 182 Forged or Rolled Alloy and Stainless Steel Pipe Flanges, Forged Fittings, and Valves and Parts for High-Temperature Service Grade F904L (Austenitic Stainless Steels) Chemical Requirements: Composition, %, max C: 0.020 Mn:2.00 P: ≤0.040 S: ≤0.030 Si: 1.00 Cr: 19.0-23.0 Ni:23.0-28.0 Mo: 4.0-5.0 Cu:1.00-2.00 N: 0.10 Austenitizing/Solutioning Temperature: 1040 °C – 1150℃ Cooling Media: Liquid Quenching Cool Below ℃ 260…

ASTM A 182 F48

ASTM A 182 Forged or Rolled Alloy and Stainless Steel Pipe Flanges, Forged Fittings, and Valves and Parts for High-Temperature Service Grade F48 (Austenitic Stainless Steels) Chemical Requirements: Composition, %, max C: 0.030 Mn:2.00 P: ≤0.045 S: ≤0.030 Si: 0.75 Cr: 17.0-20.0 Ni:13.5-17.5 Mo: 4.0-5.0 N: 0.10-0.20 Austenitizing/Solutioning Temperature, min: 1040 °C Cooling Media: Liquid Quenching Cool Below ℃ 260 Tensile…

A312 UNS N08904

ASTM A 312 Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes UNS Designation N08904 Chemical Requirements: Composition, %, max C: 0.020 Mn:2.00 P: ≤0.040 S: ≤0.030 Si: 1.00 Cr: 19.0-23.0 Ni:23.0-28.0 Mo: 4.0-5.0 N: 0.10 Cu: 1.00-2.00   Heat Treating Temperature: 1100 °C   Tensile Requirements Tensile Strength, min.: 490MPa Yield Strength, min.: 215MPa Elongation in 2…

A312 UNS S31726

ASTM A 312 Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes UNS Designation S31726 Chemical Requirements: Composition, %, max C: 0.03 Mn:2.00 P: ≤0.040 * S: ≤0.030 Si: 1.00 Cr: 17.0-20.0 Ni:14.5-17.5 Mo: 4.0-5.0 N: 0.10-0.20 Cu: 0.75 *For welded pipe, the phosphorus maximum shall be 0.045 %. Heat Treating Temperature: 1040 °C Tensile Requirements Tensile Strength,…

ASTM A240 type 410

ASTM A240/A240M Standard Specification for Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications. Type: 410 UNS Designation : 41000 Chemical Composition Requirements, %, Max. C: 0.08-0.15 Mn: 1.00 P: 0.040 S: 0.030 Si: 1.00 Cr: 11.5-13.5 Ni: 0.75 Mechanical Test Requirements Tensile Strength, min: 450Mpa Yield Strength,…

A105 DN1150 girth flanges and A516 GR.70 elliptical heads are delivered.

Item Description of goods Quantity 1 Girth Flange OD=1280, ID=1150, Thk.= 45, ASTM A105, Machined as per the drawing provided. 2 2 Girth Flange OD=1280, ID=1150, Thk.= 55, Machined as per the drawing provided. 4 3 Girth Flange OD=1280, ID=1150, Thk.= 60, Machined as per the drawing provided. 2 4 Dished Head Ellip. 2:1, ID=1150mm, T= 10mm (Min) seamless, heat treated as per ASME Sec VIII Div.1, UCS-56 and time /temperature chart along with heat treatment report will be provided. 2