Identification Symbol: A182 F60
UNS Designation: S32205
Type: Ferritic – Austenitic Stainless Steel
Heat Treatment: Solution Treat and Quench
Chemical Requirements Composition, max, %
| Elements | A182 F60 |
| Carbon | 0.030 |
| Manganese | 1.50 |
| Phosphorus | 0.030 |
| Sulfur | 0.020 |
| Silicon | 1.00 |
| Nickel | 4.5-6.5 |
| Chromium | 22.0-23.0 |
| Molybdenum | 3.0-3.5 |
| Nitrogen | 0.14-0.20 |
Tensile and Hardness Requirements
| Grade Symbol | F60 |
| Tensile Strength,min, ksi [Mpa] | 95[655] |
| Yield Strength, min,ksi [MPa] | 65[450] |
| Elongation in 2 in.[50 mm] or 4D,min, % | 25 |
| Reduction of Area, min, % | 45 |